All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Laguna Clay's Glacier Slip 100.00
Add Amount
Cornflower Blue Stain Mix (see below) 1.00

Instructions

Originally published in the May 2018 issue of Ceramics Monthly.
Cornflower Blue Stain Mix: 10% Mason Stain #6318 and 90% Mason Stain #6306.

Add 1% stain mix for Cornflower Blue. With Laguna Glacier Slip I can use a lower percentage of stain mix. When mixing my own casting slip, I generally double the amount of stain.