All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3110 80.00
EPK Kaolin 20.00
Add Amount
Bentonite 2.00
Mason Stain 6271 Mint Green 10.00

Instructions

Published in "Raku Color and Opacity" by Jeff Zamek, in theJul/Aug 2007 issue of Pottery Making Illustrated.