All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 8.00
Talc 2.00
Whiting 7.00
Zinc 5.00
Kona F-4 Feldspar 48.00
Kaolin 9.00
Flint 21.00
Add Amount
Yellow Stain 15.00

Instructions

Published in "Keisuke Mizuno" in the Nov 2000 issue of Ceramics Monthly.