All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 35.00
Minspar 200 Feldspar 40.00
OM 4 Ball Clay 15.00
SIlica 10.00

Instructions


This is a good all-around, stable glaze that can be applied via dipping, brushing, or pouring. Mix to the consistency of 2% milk.

This recipe was shared by Naomi Clement in the November/December 2019 issue of Pottery Making Illustrated.