All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 13.00
Whiting 8.70
Custer Feldspar 60.90
Kaolin 8.70
Silica 8.70
Add Amount
Red Iron Oxide 11.50

Instructions

Dull brown by itself; gives excellent results underneath cream gloss and light blue.

Published in "School and Beyond" by Andy Cantrell, in the May 2000 issue of Ceramics Monthly.