Casting Slip Moloney Hi
You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, subscribe right now for as low as $1.99/month.
Yes, I want to subscribe to Ceramics RecipesWe understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, subscribe right now for as low as $1.99/month.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Subscribe
Ingredients
Instructions
Published in "Lows-to-Mid-Range" by YunWook Mun, in the May 2014 issue of Ceramics Monthly.
I mix the water and the Darvan then add the dry ingredients. I add the stain last. The parts of the recipe are all in pounds.
It takes 5-10 minutes to cast depending on object's size and the dryness of the mold. This slip can be fired to cone 10 but after cone 6, the color is less intense.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes