All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
C-Red (Carbondale Clay) 100.00

Instructions


Mix to a light cream consistency and apply at stiff leather hard. Can be thinned to skim-milk consistency and applied to bisque ware. Slip can be dipped, poured, or brushed. I prefer to brush on multiple coats with overlapping brushstrokes.

This recipe was shared by Seth Charles in the March 2021 issue of Ceramics Monthly.