All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wollastonite 20.00
Zinc Oxide 8.00
Ferro Frit 3134 21.00
Spodumene 11.00
EPK Kaolin 20.00
Silica 20.00

Instructions


I use this as a clear glaze and as a base glaze with added colorants. This recipe was developed by Jeff Campana. Found in The Complete Guide to Mid-Range Glazes by John Britt, Sterling Publishing, 2014.

This recipe was shared by Jackie Head in the March 2019 issue of Ceramics Monthly.