All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Flint 25.56
Custer Feldspar 38.34
Whiting 13.77
Magnesium Carbonate 3.97
Barium Carbonate 4.59
Colemanite 8.44
EPK 5.33
Add Amount
Rutile 4.96
Copper Carbonate 1.86

Instructions

This is a glaze from Susan Harris (Southern Utah University).

The test tile is B-Mix fired in reduction.
This glaze tends to run if applied thickly.