All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Borax (in parts) 1.00
Water (in parts) 4.00

Instructions


Use hot water to dissolve the borax. It will recrystallize as it cools; this is fine, the crystals give a speckled effect.

This recipe was shared by Marty Fielding in the in the December 2020 issue of Ceramics Monthly.