All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 15.00
Grolleg Kaolin 20.00
Helmer Kaolin 65.00

Instructions

Published in "Blair Meerfeld" by Marty Mitchell, in the Feb 2000 issue of Ceramics Monthly.
Apply to Greenware