All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 18.00
Strontium Carbonate 13.00
Wollastonite 7.00
Nepheline Syenite 26.00
EPK Kaolin 9.00
Silica (325 mesh) 27.00
Add Amount
Mason Stain Black 6600 7.00

Instructions

Published in "Reserved for Special Occasions" in the January/February 2016 issue of Pottery Making Illustrated.