All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium Carbonate 40.00
Nepheline Syenite 45.00
Spodumene 10.00
Silica 5.00
Add Amount
Bentonite 2.00
Copper Carbonate 6.00

Instructions

I don't have source information on this glaze.

The test tile is Coleman Porcelain fired in oxidation.

Not intended for food surfaces!
Not food-safe.