All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 20.00
Potash Feldspar 40.00
EPK Kaolin 10.00
Silica 30.00
Add Amount
Yellow Iron Oxide 2.00

Instructions

Published in "Gemstones & Glazes" by Ryan Coppage, in the Sep 2017 issue of Ceramics Monthly.

 
*I suggest G200 or Custer as the most potassium-rich feldspar substitutes. Both are approximately 10:3 K2O:Na2O and are predominantly potassium oxide feldspars.