All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Sawdust Ash (washed) 10.00
Talc 5.00
Emene Clay (sieved) 25.00
Granite 60.00
Add Amount
Red Iron Oxide 4.00

Instructions

Published in "Awka Oil-Spot Glaze" by Emman Okunna, in the Feb 2000 issue of Ceramics Monthly.