All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 50.00
Wood Ash 50.00

Instructions

This recipe was contributed by Elena Renker in the November 2019 issue of Ceramics Monthly.
This slip has been applied over the glaze rather than underneath it like other slips.