All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Pine Ash 33.30
Potash Feldspar 33.30
Kaolin 33.40

Instructions


Apply thin by dipping or pouring in and out if just used as liner, and fire to cone 10 in a wood kiln with heavy reduction. I use this glaze to show iff brushwork underneath. Fly ash from a wood firing has little effect on this glaze.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.