All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 24.30
Lithium Carbonate 7.50
Custer Feldspar 24.30
EPK Kaolin 6.50
OM 4 Ball Clay 18.70
Silica 18.70
Add Amount
Yellow Ochre 9.40
Cobalt Oxide 1.00
Rutile 3.00

Instructions

Published in the March 2018 issue of Ceramics Monthly.

This recipe is from John Britt’s book, The Complete Guide to Mid-Range Glazes. The recipe was altered with progressive additions of cobalt oxide, rutile, and ash