All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
EPK 2.70
Silica 19.70
Custer Feldspar 46.10
Whiting 8.20
Dolomite 5.90
Gerstley Borate 13.50
Zinc Oxide 3.90
Add Amount
Cobalt Carbonate 1.00
Copper Carbonate 4.00

Instructions

I would assume that the source of this glaze was from Alfred University but I received this version from Shane Christensen (Dixie State University).

The test tile is Coleman Porcelain fired in reduction.
Can be runny if applied thickly.