All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 17.20
Custer Feldpsar 47.31
EPK Kaolin 19.36
Silica 16.13
Add Amount
Zinc 7.53

Instructions


This recipe is a revision of Hansen Charcoal Matte Black with increased silica. I substituted Forshammer feldspar (a Swedish feldspar) for the Custer feldspar. Shown with 1% titanium dioxide.

This recipe was shared by Alisa Liskin Clausen in the May 2019 issue of Ceramics Monthly.