All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 20.00
OM 4 Ball Clay 20.00
6 Tile Kaolin 60.00

Instructions


Apply thin via dipping or brushing. Fires red to buff.

This recipe was shared by Trevor Youngberg in the April 2020 issue of Ceramics Monthly.