All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
soda ash 50.00
Ball Clay 50.00

Instructions

Add small percentages of oxides and carbonates for different colored shinos. 

 

This recipe was shared by Dan Anderson in the March 2022 issue of Ceramics Monthly.