All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wollastonite 20.00
Cuter Feldspar 20.00
Ferro Frit 3134 20.00
EPK Kaolin 20.00
Silica 20.00
Add Amount
Degussa Orange 239616 2.00

Instructions

Published in "Technofile Ceramic Stains" by John Britt, in the February 2013 issue of Ceramics Monthly.