All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wollastonite 20.00
Custer Feldspar 20.00
Ferro Frit 3134 20.00
EPK Kaolin 20.00
Silica 20.00
Add Amount
Praseodymium Yellow 6433 4.00

Instructions

Published in "Technofile Ceramic Stains" by John Britt, in the February 2013 issue of Ceramics Monthly.