All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Strontium Carbonate 27.81
Whiting 11.00
Ferro Frit 3110 16.68
EPK Kaolin 9.50
Silica 35.01
Add Amount
Red Iron Oxide 0.50

Instructions

Published in "Exploring Glazes: From Perfect fit to Crackle and Matte," in the March 2016 issue of Ceramics Monthly.

The image shown here has multiple glazes on it, including #24 Crackle Clear (Currie Strontium Series) with 0.5 % Red Iron Oxide added to it, which gives it a water blue color.
A bit of Iron seems to make it melt better.