Recipe Tags: Spanish Red Iron Oxide

Lung Chuan Celadon for Reduction Cooling

Lung Chuan Celadon for Reduction Cooling

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 9-10

Atmosphere: Reduction

Surface Finish: Glossy

Color: Blue

Sprite Bottle Green 04

Sprite Bottle Green 04

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 04-03

Atmosphere: Oxidation

Surface Finish: Glossy

Color: Green

Blue Celadon

Blue Celadon

4 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 54 votes, average: 4.25 out of 5 (4 votes, average: 4.25 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10-11

Atmosphere: Reduction

Surface Finish: Glossy

Color: Blue celadon

Green Celadon

Green Celadon

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 10

Atmosphere: Reduction, Soda

Surface Finish: Glossy

Color: Light green

Floating Blue Glaze

Floating Blue Glaze

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Glossy

Color: Medium blue

Ketchup Red

Ketchup Red

0 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 50 votes, average: 0.00 out of 5 (0 votes, average: 0.00 out of 5)
You need to be a registered member to rate this.

Firing Temperature: Cone 6

Atmosphere: Oxidation/Neutral

Surface Finish: Matte

Color: Medium red