In a fuel-burning kiln, air that feeds initial combustion; in a wood-burning kiln, air that feeds base of flames; in a gas kiln air that enters back end of burner tube in an atmospheric burner, or via blower in a power burner. See secondary air.
Source: Clay: A Studio Handbook