Exhibition Dates: October 17–December 12, 2019

Bottoms Up! An Online Juried Exhibition Featuring Cups

Caleb Zouhary, Best in Show

Title: Rainbow Stein, Price: $58, Materials: Porcelain Mug, Shino Base Glaze, Layered Rainbow and Microcrystalline Cobalt Glaze, Firing Temperature: cone 10, Electric, Dimensions: 5.5”  x  5” x 4”, Date Completed: 2019     

Andrea Lynn Stocker, Runner Up

Title: Coral 2, Price: NFS, Materials: Slip-Cast Porcelain, Hand-built Black Porcelain Coral, Clear Liner Glaze, Firing Temperature: cone 6, Soda Kiln, Dimensions: 6″ x 4.5″ x 6.5″, Date Completed: 2018

FINALISTS

Eliza Wang, Title: Tea Time, Price: NFS, Materials: Porcelain Clay, Firing Temperature: Cone 10, Wood Fired, Dimensions: 4.5” x 2.5”, Date Completed: 2019

Will Talbot, Title: Ocean Guinomi, Price: NFS, Materials: Porcelain, Firing Temperature: Cone 10, Soda Fired, Dimensions: 2 x 2.5 x 2.5, Date Completed: 2019

Emily Rangel-Cascio, Title: One Cannot Exist Without the Other, Price: NFS, Materials: Porcelain and Gold Luster Firing, Temperature: Cone 6 Oxidation, Dimensions: 10” X 7” X 8”, Date Completed: 2018

Heidi Tarver, Title : Pink Espresso Cup and Saucer, Price: $80, Materials: Hand Colored Porcelain, Firing Temperature: Cone 5

Heather Ossandon, Title: Other View of 2 Mugs, Price: NFS, Materials: Stoneware, Firing Temperature: Cone 10, Wood Fired, Dimensions: 5” (with handle) x 6.25”, Date Completed: 2019

Jason Sonsthagen, Title: Dissolving Crystals, Price: $70 Materials: Porcelain, Firing Temperature: Cone 10, Gas Reduction, Dimensions: 6” x 3.75”, Date Completed: 2018

Pamela Ivanković, Title : Vesselfinder Free, Price: NFS, Materials: Handmade White Clay, Mat Glazed, Firing Temperature: Cone 1060, Dimensions: 27 cm x 22 cm, Date Completed: 2019

Jennifer Fujimoto, Title: Tea Doll, Price: NFS, Materials: Stoneware with Underglaze Decoration and Glazes, Firing Temperature: Cone 6, Electric Kiln, Dimensions: 4.25” x 4.25” x 7," Date Completed: 2019

Andrew Clark, Title: Cup with Drink Counter, Price: NFS, Materials: Stoneware, Terra Sig, Underglaze, Glaze, Firing Temperature: Cone 6

Dodie Campbell, Title: Pair of Cups, Price: $65, Materials: Stoneware, Firing Temperature: Cone 6 Reduction

Lauren Kearns, Title: Cup, Price: NFS, Materials: Grolleg Porcelain, Underglazes with Clear Glaze, Firing Temperature: Cone 9, Dimensions: 3.5" x 3" Date Completed: 2017



Ann Ruel, Title: Woodpecker, Price: NFS Materials: Porcelain, Underglazes, Glazes, Firing Temperature: Cone 5, Electric, Dimensions: 5" x 3" Date Completed: 2019

Tony Young, Title: RIOT Tumbler, Price: $70, Materials: Stoneware, Underglaze, Glaze, Slipcast, Firing Temperature: cone 5, Dimensions: 3 x 6.25”, Date Completed: 2019

Christopher Williams, Title: Mug and Hand, Price: $100, Materials: Low-fire Earthenware, Majolica, Underglaze, Glaze, Glass, Firing Temperature: NA, Dimensions: 3.5" x 5" x 3", Date Completed: NA

Title: Copper Blush Dragon Flower Mug, Price: $70, Materials: Thrown, Altered, and Textured Porcelain, Interior Copper Glaze, Firing Temperature: cone 7, Soda Fired, Dimensions: 4.5” x 4.5” x 3.25”, Date Completed: 2019

Shana Salaff, Title: Cup 3, Price: $35, Materials: Porcelaneous Stoneware, Firing Temperature: cone 5, Oxidation, Dimensions: 4.5” x 3” x 3”, Date Completed: 2019

Marcia Friedman, Title: Soda Flash Teabowl, Price: NFS, Materials: Columbia White Firing Temperature: cone 10, Soda Reduction, Dimensions: 3.5" x 3.0", Date Completed: 2018

Jan Schachter, Title: Teabowl with Pink Rim, Price: $80, Materials: Porcelain, Firing Temperature: Cone 10-11, Wood Fired, Dimensions: 3" x 4" x 4", Date Completed: 2008

Visit Eliza Wang's ICAN Artist Portfolio here!

Visit Will Talbot's ICAN Artist Portfolio here!

Visit Lauren Kearns's ICAN Artist Portfolio here!

Visit Ann Ruel's ICAN Artist Portfolio here!

Visit Jan Schacter's ICAN Artist Portfolio here!