ICAN Online Exhibitions provide the perfect opportunity for ICAN members to show their work to a growing, international audience of ceramics enthusiasts! Contest finalists are featured here, on the Ceramic Arts Network website, for an 8-week exhibition while being promoted by ICAN to our global network of potters and sculptors. Each winning piece may be offered for sale through the exhibition website. ICAN Online Exhibitions, held twice a year, are open to active ICAN members only. To learn more about ICAN Online Exhibitions, browse the FAQ .

Drum roll please . . . .

The winners of the 3rd Annual ICAN Holiday Cup Show are:

BEST IN SHOW: Andrew Geithner

Austin Geithner - BEST IN SHOW: Autumnal Cup, 3.5 in. (9 cm) in height, Standard 257 porcelain, multiple glazes sprayed and layered,  fired to cone 10 in an electric kiln, 2022.

Runner Ups

Ishara Sweeney - FIRST RUNNER UP: Capricorn, white stoneware, 5 in. (13 cm) in diameter, underglaze, fired to cone 6, gold luster, 2022. Julie Woodrow - SECOND RUNNER UP: Bee Rhyton (with stand and funnel), 8 in. (20 cm) in width, white stoneware, Amaco Velvet underglazes, clear glaze, fired to cone 6 in an electric kiln, Apoxie clay, steel wire, acrylic gouache, 2022. Photo: Mark Steele.


Honorable Mentions

Posey Bacopoulos: Cup with feet, 5 in. (13 cm) in height, terra cotta, majolica, fired to cone 04, gold and silver decals fired to cone 018, 2022. Jason Vantomme: Textured Cup 2, 4 in. (10 cm) in height, stoneware, fired to cone 6 in oxidation, 2022.

Bev Zerbib-Berda: California Redwood Twisted Mug, 5 in. (13 cm) in height, porcelain ash and tenmoku glaze, fired to cone 10 in reduction, 2022. Barry Rhodes: Tricornered Whiskey Cup with Fan Pattern,  3 in. (8 cm) in height, mid-range stoneware with underglazes, slips, underglaze pencil, custom stamps, microcrystalline glaze, fired to cone 6 in oxidation, 2022.

Brian Wildeman: Tri-color mug, 5 in. (13 cm) in height, wheel-thrown stoneware, fired to cone 6 in oxidation, 2021. Mimi Stadler: Oxblood Cup 2, 3.5 in. (9 cm) in height, porcelain with copper red glaze, fired in reduction to cone 10, 2022.


Debra Britt: Fluted tumbler with feet, 5 1/8 in. (13 cm) in height, clay, fired to cone 10 in a salt kiln, 2022. Mandy Henebry: Gold Flowers, 4.75 in. (12 cm) in height, stoneware, black colored clay, premium gold luster, fired to cone 5, 2022. 
 
Jennifer Rosseter: Wild Child demi-tasse cup set, 3.75 in. (10 cm) in width, stoneware, underglaze, underglaze transfer, glaze, fired to cone 5 in an electric kiln, 2022. Dee Harris: His’n’Hers, to 5.5 in. (14 cm) in height, Laguna porcelain, black underglaze with sgrafitto decoration, glaze, fired to cone 10/11 in a soda kiln, 2022.
 
 