Techno File: Porcelain Bodies 201
Need a good porcelain clay body recipe, but having trouble choosing from the hundreds online? Here are some important rules … Read More
Al2O3×4SiO2×H2O—used in HT claybodies (20% or less) to reduce thermal expansion, increase thermal shock resistance, reduce shrinkage, give stronger vitreous bodies. May reduce plasticity. Source: Clay: A Studio Handbook
Need a good porcelain clay body recipe, but having trouble choosing from the hundreds online? Here are some important rules … Read More
One of my favorite things about ceramics is that there seem to be endless ways to decorate clay surfaces. In … Read More
Combining the right materials within acceptable limits to make a workable clay body can be difficult and full of trial … Read More