Tag: pinholing

Glaze defect characterized by fine pinholes in the surface—often caused by pinholes already present in dry unfired glaze coating. Can also be caused by burst bubbles in glaze surface that are not given opportunity to “heal” at end of firing. Source: Clay: A Studio Handbook