Laboratory device for measuring specific gravity in slips and glazes. Does not give absolute measurement, and should be used only for comparing and reproducing results. Must be an appropriate glaze hydrometer for measuring suspensions heavier than water. Does not work well in thick glazes. Source: Clay: A Studio Handbook
Vase, 14 in. (36 cm) in length, Polseno Peach and Polseno Terra Cotta with additional glazes.
I am not sure when … Read More
Underfired glazes are usually matte and dry and can feel rough. Some gloss glazes seem like they were properly fired … Read More