Laboratory device for measuring specific gravity in slips and glazes. Does not give absolute measurement, and should be used only for comparing and reproducing results. Must be an appropriate glaze hydrometer for measuring suspensions heavier than water. Does not work well in thick glazes. Source: Clay: A Studio Handbook