Susan Beiner’s Garden of UN-Earthly Delights
Susan Beiner’s installations present a hybrid, often vibrantly colored world saved by an ecosystem able to adapt to and evolve … Read More
Action of a solvent material on a solid, bringing it into liquid solution. Source: Clay: A Studio Handbook