Glazes in the Chun glaze family are lovely light blue high fire glazes that feature opalescence caused by micro bubbles … Read More
A pale gray-blue feldspathic stoneware glaze featuring opalescence due to inclusions of phosphorous and/or other materials. Source: Clay: A Studio Handbook