Ceramic luster glaze is an overglaze that comes in a variety of finishes (including gold, silver, platinum, and mother of … Read More
Metallic overglaze finish created either by painting prepared luster (metallic salt in organic binder) over previously fired glaze and firing to cone 018 or by spraying metallic salt dissolved in water into kiln and/or on to wares at low red heat, either during cooling cycle of a glaze-firing, or in a separate firing heated to that temperature. Source: Clay: A Studio Handbook