2019 ICAN Online Juried Exhibition: Bottoms Up!

Details:

2019 ICAN Online Juried Exhibition: Bottoms Up!
1st annual ICAN Online Juried Exhibition
October 17th–December 12th, 2019


Caleb Zouhary,
Best in Show

Title: Rainbow Stein
Materials: Porcelain Mug, Shino Base Glaze, Layered Rainbow and Microcrystalline Cobalt Glaze
Firing Temperature: Cone 10, Electric
Dimensions: 5.5”  x  5” x 4”
Date Completed: 2019

 


Andrea Lynn Stocker,
Runner Up

Title: Coral 2
Materials: Slip Cast Porcelain, Hand-built Black Porcelain Coral, Clear Liner Glaze
Firing Temperature: Cone 6, Soda Kiln
Dimensions: 6″ x 4.5″ x 6.5″
Date Completed: 2018

 


FINALISTS

 

Eliza Wang

Title :Tea Time
Materials:
Porcelain Clay
Firing Temperature: Cone 10, Wood Fired
Dimensions: 4.5” x 2.5”
Date Completed: 2019

Will Talbot

Title: Ocean Guinomi
Materials:
Porcelain
Firing Temperature: Cone 10, Soda Fired
Dimensions: 2 x 2.5 x 2.5
Date Completed: 
2019

 

Emily Rangel-Cascio

Title: One Cannot Exist Without the Other
Materials:
Porcelain and Gold Luster
Firing Temperature: Cone 6 Oxidation
Dimensions: 10” X 7” X 8”
Date Completed: 2018

Jason Sonsthagen

Title: Dissolving Crystals
Materials: 
Porcelain
Firing Temperature: Cone 10, Gas Reduction
Dimensions: 6” x 3.75”
Date Completed: 
2018

 

Heidi Tarver

Title : Pink Espresso Cup and Saucer
Materials:
Hand Colored Porcelain
Firing Temperature: Cone 5
Dimensions: 2″ x 4″ x 4″
Date Completed: NA

Heather Ossandon

Title: Other View of 2 Mugs
Materials: 
Stoneware
Firing Temperature: Cone 10, Wood Fired
Dimensions: 5”(with handle) x 6.25”
Date Completed: 
2019

 

 

 

Pamela Ivanković

Title : Vesselfinder Free
Materials:
Handmade White Clay, Mat Glazed
Firing Temperature: Cone 1060
Dimensions: 27 cm x 22 cm
Date Completed: 2019

Jennifer Fujimoto

Title: Tea Doll
Materials: 
Stoneware with Underglaze Decoration and Glazes
Firing Temperature: Cone 6, Electric Kiln
Dimensions: 4.25” x 4.25” x 7”
Date Completed: 
2019

 

Andrew Clark

Title : Cup with Drink Counter
Materials:
Stoneware, Terra Sig, Underglaze, Glaze
Firing Temperature: Cone 6
Dimensions: 4″
Date Completed: 2019

Dodie Campbell

Title: Pair of Cups
Materials: 
Stoneware
Firing Temperature: Cone 6, Reduction
Dimensions: 3″ x 3″ x 3″
Date Completed: 
2019

 

 

Lauren Kearns

Title : Cup
Materials:
Grolleg Porcelain, Underglazes with Clear Glaze
Firing Temperature: Cone 9
Dimensions: 3.5″ x 3″
Date Completed: 2017

Ann Ruel

Title: 
Woodpecker
Materials: 
Porcelain, Underglazes, Glazes
Firing Temperature: Cone 5, Electric
Dimensions: 5″ x 3″
Date Completed: 
2019

 

Tony Young

Title: RIOT Tumbler
Materials:
Stoneware, Underglaze, Glaze, Slipcast
Firing Temperature: Cone 5
Dimensions: 3 x 6.25”
Date Completed: 2019

Christopher Williams

Title: Mug and Hand
Materials: 
Low-fire Earthenware, Majolica, Underglaze, Glaze, Glass
Firing Temperature: NA
Dimensions: 3.5″ x 5″ x 3″
Date Completed: NA

 

Lora Rust

Title: Copper Blush Dragon Flower Mug
Materials: 
Thrown, Altered, and Textured Porcelain, Interior Copper Glaze
Firing Temperature: Cone 7, Soda Fired
Dimensions: 4.5” x 4.5” x 3.25”
Date Completed: 
2019

 

Shana Salaff

Title: Cup 3
Materials: 
Porcelaneous Stoneware
Firing Temperature: Cone 5, Oxidation
Dimensions: 4.5” x 3” x 3”
Date Completed: 
2019

Marcia Friedman

Title : Soda Flash Teabowl
Materials:
Columbia White
Firing Temperature: Cone 10, Soda Reduction
Dimensions: 3.5 x 3.0
Date Completed: 2018

Jan Schachter

Title : Teabowl with Pink Rim
Materials:
Porcelain
Firing Temperature: Cone 10-11, Wood Fired
Dimensions: 3 x 4 x 4
Date Completed: 2008

 

 

 

 

 

 

 


Juror: Jessica Knapp, Ceramics Monthly Editor

Juror’s Biography

Jessica Knapp was born and raised near Philadelphia, Pennsylvania. She received a Bachelors of Fine Arts and a Bachelor of Arts from Kutztown University, Kutztown, PA, followed by a year of post-baccalaureate study at Virginia Commonwealth University. She received her Masters of Fine Arts degree in ceramics at the University of Colorado at Boulder in December 2003. From 2004 to 2006, she was a volunteer studio technician and artist in residence at San Diego State University. She was an artist in residence at the Ceramic Center Berlin from 2006 to 2007, funded by a German Chancellor Scholarship awarded by the Alexander von Humboldt Foundation. She currently lives and works in Columbus, Ohio.