15 Tried and True Cone 6 Glaze Recipes: Recipe Cards for our Favorite Mid-Range Pottery Glazes

Get recipes and learn about testing procedures for mid-range glazes in this FREE PDF!

Good news cone 6 potters! We’ve gathered some of our favorite cone 6 glaze recipes in a convenient recipe-card format, perfect for printing and taking to the pottery studio. If you are interested in building a collection of beautiful cone 6 pottery glazes, you’ve found the perfect resource. If you’ve been low firing and would like to turn up the heat a bit, here’s a great assortment of cone 6 recipes to start with. Or if you have grown bored with your current cone 6 glazes, try out a few of these. There is something for everyone involved in ceramics, so download your free copy of 15 Tried and True Cone 6 Glaze Recipes: Recipes and Testing Procedures for our Favorite Mid-Range Pottery Glazes when you sign up for Ceramic Arts Daily today!

Check out this excerpt:

How to test Cone 6 Glaze Recipes for Color Response and Surface Texture

by Yoko Sekino-Bove

There are so many wonderful books, websites and even software that feature spectacular glaze formulas; so one may wonder why this article should be introduced to you. The focus of this research was to establish a comprehensive visual library for everyone. Rather than just providing the reader with a few promising glaze formulas, this reference is a guideline.

Because it is a guide, there are some test tiles that do not provide immediate use other than the suggestion of what to avoid, or the percentages of certain chemicals that exceed the safe food-serving level, etc., but I believe that this research will be a good tool for those who wish to experiment with, and push the boundaries of, mid-range firing.

Many people may be thinking about switching their firing method from high-fire to mid-range. For instance, students who recently graduated and lost access to school gas kilns, people with a day job and those who work in their garage studios, or production potters who are concerned about fuel conservation and energy savings. This reference is intended as a tool for those people to start glaze experimentations at mid-range that can be accomplished with minimal resources.

There is no guarantee that this chart will work for everyone everywhere, since the variety between the different resources overwhelmingly affects the results, but by examining a few glazes in this chart you can speculate and make informed adjustments with your materials. This is why all the base glazes for this research use only simple materials that are widely available in the US.

Five years ago, when I was forced to switch to mid-range oxidation firing with an electric kiln, from gas-fueled reduction firing at high temperatures, most of my hard-earned knowledge in high-fire glazes had to be re-examined. Much to my frustration, many earth metal colorants exhibited completely different behaviors in oxidation firing. Also, problems in adhesion were prominent compared to high-fire glazes.

The role of oxides and carbonates used for texturing and opacifying were different as well. But compiling the available glazes and analyzing them were not enough. I felt there should be a simple chart with visual results that explained how the oxides and carbonates behave within this firing range. This motivated me to write a proposal for glaze mid-range research to the McKnight Foundation, which generously sponsors a three-month artist-in-residence program at the Northern Clay Center in Minneapolis, Minnesota.

Most of the tests presented in these experiments were executed at the Northern Clay Center from October to December in 2009 using clay and dry materials available at Continental Clay Co. The rest of the tests were completed after my residency at my home studio in Washington, Pennsylvania. For those tests, I used dry materials available from Standard Ceramics Supply Co.

Test Conditions

Clay body: Super White (cone 5–9) a white stoneware body for mid-range, commercially available from Continental Clay Co.

Bisque firing temperatures: Cone 05 (1910°F, 1043°C), fired in a manual electric kiln for approximately 10 hours.

Glaze firing temperatures: The coloring metals increment tests (page 50) were fired to cone 5 (2210°F, 1210°C) in a manual electric kiln for approximately 8 hours. The opacifier/texture metals increment tests (page 51) were fired to cone 5 in an automatic electric kiln for 8 hours.

Glaze batch: Each test was 300g, with a tablespoon of epsom salts added as a flocculant.

Glazing method: Hand dipping. First dip (bottom half): 3 seconds. Second dip (top half) additional 4 seconds on top of the first layer, total 7 seconds.

Coloring Metals Increment Chart

The following colorants were tested: black nickel oxide, cobalt oxide, copper carbonate, chrome oxide, iron chromate, manganese dioxide, red iron oxide, rutile, and yellow ochre. You should note that tests with cobalt oxide and chrome oxide in high percentages were not executed due to the color predictability. Other blank tiles on the chart are because either the predictability or the percentages of oxides are too insignificant to affect the base glazes.

Depending on firing atmospheres, manganese dioxide exhibits a wide variety of colors. When fired in a tightly sealed electric kiln with small peepholes, the glaze color tends toward brown, compared to purple when fired in a kiln with many and/ or large peepholes.

Please note that some of the oxides and carbonates in this test exceed the safety standard for use as tableware that comes in contact with food. Check safety standards before applying a glaze with a high percentage of metal oxides to food ware and test the finished ware for leaching.

Test tile numbering system: The glaze name is the first part of the identification number, followed by an abbreviation or code that stands for the colorant name. The last part is a two or three digit number referring to the percentage of colorant added. So, for example if a test was mixed with glaze base N501, to which 1 percent cobalt oxide was added, the test tile marking would be: N501COX10.

Conclusion

This group of tests has been a great opportunity for me to study the characteristics of oxides and carbonates and how they behave at mid-range temperatures. There are scientific methods for calculating glazes and proven theories, but there are many small pieces of information that can only be picked up when you actually go through the physical experiments. It is important for us to become familiar with a glaze’s behavior so that we can better utilize it. Key to that is learning both the theory and application. It is my hope that these tests will benefit many potters by helping them to expand their palette and inspire them to test the possibilities.

the author Yoko Sekino-Bové is an artist living in Washington, Pennsylvania. She would like to thank the McKnight Foundation and the Northern Clay Center and its supporting staff for making this research possible. 

How to test Cone 6 Glaze Recipes for Color Response and Surface Texture

by Yoko Sekino-Bove

A great place to start experimenting is with these five great recipes, from glossy to
matte, which have already been tested and are presented in chart form.

Blue Green/Copper Red Glaze

Cone 6 oxidation or reduction

From Rick Malmgren, Ceramics Monthly, October 2000

Wright’s Water Blue Glaze

Cone 6 oxidation or reduction

From David Wright, Ceramics Monthly, April 1998

Basic Bronze

Cone 6 oxidation

From A. Blair Clemo, Ceramics Monthly, December 2013

Fake Ash Glaze

Cone 6 reduction

From Diana Pancioli, Ceramics Monthly, June 2006

Strontium Crystal Magic—Warm and Cool

Cone 6 oxidation

From Steven Hill, Ceramics Monthly, March 2012

Temmoku

Cone 6 reduction

From Rick Malmgren, Ceramics Monthly, October 2000

Marilee’s Lava

Cone 6 oxidation or reduction

From Rick Malmgren, Ceramics Monthly, October 2000

Eggshell

Cone 6 oxidation

From Central Carolina Community College, Ceramics Monthly, October 2004

Textured Blue

Cone 6 reduction

From Diana Pancioli, Ceramics Monthly, June 2006

Download the free guide right now, and become a better ceramic artist tomorrow. That’s our promise to you from Ceramic Arts Network!

Best regards,

Jennifer Poellot Harnetty
Editor, Ceramic Arts Daily

PS: Remember, the artists featured on Ceramic Arts Network are among the top ceramic artists in the world today, who excel in everything from functional pottery to abstract ceramic sculpture. When you download one of our free guides, you get the best possible advice available and you become a part of our community – enjoying our artists’ stories, gaining inspiration from their work and finding confidence to try new techniques every day!

PPS: Even if you’re not brand new to clay, this guide is bound to have some tips in it that you’ve never heard before – and remember, it’s absolutely FREE, so why wouldn’t you read it today?

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend