How to Make Custom Clay Extruder Dies with Old Credit Cards

Another great way to put old credit cards to use in the pottery studio: make your own extruder dies!

extruderdie-695

Chances are, if you have a mailbox, it is filled to the brim every day with direct mail credit card offers. Or maybe you have a few expired gift cards laying around. You have probably heard that these and other retired credit cards can be put to use in the ceramics studio as throwing ribs. 

But today, ceramic artist Daryl Baird presents another great use for these throw-away items: custom clay extruder dies! Way to go Daryl! – Jennifer Poellot Harnetty, editor.


Personalize Your Extrusions with Custom Clay Extruder Dies

 What You’ll Need to Make Clay Extruder Dies:

  • Number 2 pencil
  • Indelible marker with a fine point
  • Dremel tool and assorted bits
  • X-Acto knife and several No. 11 blades
  • Emory cloth or 150-grit sandpaper
  • Rubbing alcohol and a small rag

Safety glasses or goggles are essential when using the Dremel tool. Optional tools include a hand drill and bits, a scroll saw, a jeweler’s saw and a small vise.

Clay Workshop Handbook

Learn techniques from the pros when you download this freebieClay Workshop Handbook.



The Process

To begin, use a No. 2 pencil with a good eraser to lay out the shape of the extruder die opening. Dull the finish of the card with fine sandpaper if the pencil marks are too light. Go over the pencil drawing with a fine-point, indelible marker, like a Sharpie (figure 1). If you make a mistake, these lines can be removed by wiping the card with a rag dipped in rubbing alcohol.


 

To cut out the shape you’ve drawn, a hand-held rotary tool, like the type made by Dremel, works fast (figure 2) and is fairly easy to control. These come with a variety of drill bits, along with grinding and sanding bits that can be used to refine the shape of the opening.

In addition to using a Dremel tool, I tried cutting out the die shapes with a scroll saw. It worked well, but setting up the saw for this was tedious and time-consuming. I also gave a coping saw and a jeweler’s saw a try. Even with a fine-toothed blade installed, the coping saw was next to impossible to use. The jeweler’s saw cut more smoothly but it was slower than using a Dremel tool.

Once the opening has been cut out with the Dremel tool, it will be rough, so you’ll need to clean it up. I like using an X-Acto knife with a No. 11 blade to clean up the opening and square-up the corners (figure 3). The blades are very sharp but they dull quickly when cutting plastic. Have several on hand and change blades often.

Once you’re satisfied with the die shape, use a small piece of sandpaper or emory cloth to clean off any burrs (figure 4). I used a narrow strip cut from a foam-backed sanding pad because of the way it fits the contours and corners.

Using Your Custom Clay Extruder Dies

House number made with custom extruder dies.

Credit card clay extruder dies are best suited for use with extruders that have a 3 to 4-inch barrel. Don’t try to use credit card dies in large-barreled extruders because these types of extruders will exert too much pressure on the die, and cause it to crack. For the same reason, you’ll achieve the best results by using only a two or three pound charge of very soft, well-wedged clay in the extruder to minimize the stress placed on the die. Place the card on a clay extruder die with a hole somewhat larger than the hole you just cut. I’m using a North Star standard extruder and the outer part of a small hollow die makes an ideal mounting plate for the credit card die. Looking from the underside, make sure the die is centered (figure 5).

Hold the die in place and turn it face up. Use small wads of soft clay to anchor the credit card to the mounting plate (figure 6). Then, attach the die to the extruder barrel and load the charge of clay into the barrel carefully so the credit card does not become misaligned. Evaluate the first extrusion. If areas need to be refined, it’s easy to go back and give the shape a little “tune up.”

See how you can make an extruded baking dish and how to keep your extruder clean!

Do you have any other uses for old credit cards? Share them in the comments below!


From installation to making custom clay extruder dies, Daryl Baird doesn’t miss a step in his DVD, The Extruder Video. A little planning goes a long way, and Baird shares a multitude of tips for creating an efficient workspace and having a high success rate with your extrusions. And to get you inspired to get extruding, he walks you though a series of step-by-step projects, encouraging experimentation along the way.

Pick up your copy today!


**First published in 2008
Comments
  • Peter S.

    In addition to the above suggestions for out of date credit cards I use them as shims to keep my wheel head perfectly balanced and to shim up pieces with irregular rims for trimming.

  • Diane M.

    I’ve been taught to use them to make custom-shaped rib tools for feet, rims and surface decoration. A foot rib reduces trimming work, rim ribs create special profiles, and various beading or reeding can be easily done.

  • Carol D.

    I use a credit card to clean off the wheel head. One trimmed into a triangle to do the rough trim on the foot of a piece while it’s on the wheel. I suppose one could use a credit card as a stiff rib… cut to size and shape. Also a template for a form either on the wheel or for handbuilding. There are so many uses for these stiff plastic pieces that we often simply cut up and throw away… shaaammmmeeee…! LOL

  • I cut old credit cards up with pinking shears for use as score and slip tools in my classroom. Easy to make and certainly plentiful.

  • I’ve given several friends house warming gifts of their house number using this wonderfully easy technique.

  • Bauducco C.

    Muy simbólico!!!, me encantó! tengo alguna tarjeta vieja, y lo voy a poner en práctica

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend