An Experienced Wood Firer Shares Kiln Plans for a Small Instructional Wood Kiln

John Thies has been building, firing and maintaining large wood kilns for more than thirty years. For more than ten years he has been teaching group workshops with his 300-cubic-foot crossdraft noborigama-style kiln. But when many of his students asked for additional space in his kiln at other times during the year, which wasn’t possible with his normal production schedule, he began to brainstorm a plan for a small, efficient wood kiln that students could fire on their own.

What he came up with was the Manabigama. This sweet little kiln gives students the full wood firing experience, without disrupting John’s regular schedule. Today, he tells us about that kiln and shares his kiln plans. Plus, one of his students shares her experiences firing the kiln. – Jennifer Poellot Harnetty, editor.


I set out to build a very versatile and efficient wood-firing kiln that could be used by students who had interest in a complete hands-on experience, from the preparation, loading, firing and unloading to the final clean-up phase. I didn’t want to interfere with the successful larger firings, in which students can get a large volume of wood-fired pots without the in-depth hands-on experience. The new kiln would allow me to cut down on the extensive labor, fuel and overhead costs of my larger kiln.

manabigama_01I named the new kiln “Manabigama” at the suggestion of my friend Phil Berneburg, former technical editor for CM. In Japanese, mana means educational or learning, bi means a thing of beauty, and gama means kiln. The Manabigama is a traditional design with a few simple modifications. I see it as a cross between an anagama and a groundhog-style kiln. Basically, it is a crossdraft tube built into the side of a hill.

The overall interior dimensions are 24 inches in width, 7 feet in depth, 40 inches in height. Its firebox is in the front, incorporated into the inside with a grate system, and extra air intakes are built into the front and sides. This is done to provide more secondary air intake to help burn green or wet fuel. The firebox is plenty adequate being 2 feet wide, 2 feet deep and 30 inches high from the floor to ware level. The chimney has inside dimensions of 9 inches deep by 18 inches wide and is 12 feet high. The shape is a long rectangle with two straight, 18-inch-tall side walls and a catenary arch built on top. This creates ample headroom for ease of loading, as well as extra height for stacking and tall pieces.

A Guide to Ceramic Kilns

Find helpful tips for choosing the right kiln firing method when you download this freebieA Guide to Ceramic Kilns.

Download Today!

There is approximately 24 cubic feet of ware space, more than enough for teaching purposes. The kiln door is in front, only halfway down, and is bricked up including the stoke hole. It can be loaded in two to three hours, fires evenly to Cone 10-12 in eight hours tops, or if you choose, you can fire two to three days depending on how much ash buildup you like. The consumption of fuel is also minimal-less than half a cord of wood.

All in all, the Manabigama is a very simple design to build. It is capable of yielding wonderful ash-glazed pieces with a minimum of labor, fuel and overhead costs. And it is a fantastic wood-fired kiln for teaching without the tremendous strain of a large three-chambered kiln.

manabigama_sideview

The Manabigama kiln was constructed with one layer of firebrick, a 2-inch coating of mud and straw, and steel buttressing, which is an optional feature.

manabigama_topview

For more information on the Manbigama and to see some of John Thies’ work, visit www.monocacypottery.com.

 


THOUGHTS FROM A MANABIGAMA GUINEA PIG

by Mea Rhee

I had attended kiln workshops for several years, and felt I was ready for more. I was looking for a wood kiln that I could try to fire by myself when John called and said, “Come see my new kiln. I think you’re going to like it.” Of course I volunteered to test fire it.

I had help and John was always nearby, but for the first time I was able to manage the entire process, which was my goal for this firing. The kiln’s design is just right for a student at my level. All of its processes are small, straightforward and flexible. I love that there is no barrier between the firebox and the pots, so the pots receive as much effect from the fire as possible. This is my goal aesthetically too.

I am already busy designing pots for my next kiln load. I plan to gain as much understanding as I can each time I fire it, and enjoy every minute of it. This kiln is going to carry me to a point in the future when I’m ready to build my own. And when I get there, I’ll probably build something very similar.


**First published in November 2012
Comments
  • For the stainless steel grate bars, do they have to be solid or can heavy gauge stainless steel pipe do the trick? What kind of bars are normally used for the grates?

  • I build mostly brick ovens but would love to try one of your kilns. Not being a poster I am not getting it. Do you brick in the entrance each time you use it?

  • would so love to build one of these in my backyard here in western australia, wonder if you could use it on total fire ban days this summer, might see if some friends will help create one in the backyard, sounds great, Rae

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend