Emerging Artist 2013: Tom Jaszczak – Helena, Montana

 

Tom Jaszczak’s ceramic surfaces are deep and inviting. The combination of bold graphic lines with bright colors over subtle, earth-toned slips and atmospheric firing result in a really satisfying balance between form, line, and surface.

 

Left: Pitcher, 10 in. (25 cm) in height, wheel-thrown and altered earthenware, applied slips and underglaze, soda fired to cone 3, 2012.

 

Below: Cocktail cups, up to 3 in. (8 cm) in height, wheel-thrown and altered earthenware, applied slips and underglaze, soda fired to cone 3, 2012.

 