1 Bottle and shot glass, to 8 in. (20 cm) in length, porcelain with Blue Salt glaze, 2015.

2 Plates, to 7 in. (18 cm) in length, porcelain, Bray Shino and Oxidation Celadon glazes, 2015.

3 Mug, 5 in. (13 cm) in height, porcelain, flashing slip, and Honey Celadon glaze, 2015.

4 Yunomi, 4 in. (10 cm) in height, porcelain,Yellow Salt glaze, 2015.

5 Pitcher and cup, 11 in. (23 cm) in height, porcelain, Green and Yellow Salt glazes, 2015. All pieces fired in a reduced wood/soda kiln fired to cone 10.
Lisa York shares some of the high-fire glaze and slip recipes she uses alone, in combination, and with resist decoration on her functional pots.