1 The gravity filter press before tacking the bedsheets in place.

One of the best ways to thoroughly mix a clay body is to mix it into a slip or slurry and then dry it out. A home-built gravity filter press is an effective tool to turn that slip into a workable clay body.

While in North Carolina, this past summer as a resident artist at STARworks Center for Creative Enterprises, I was fascinated with the prevalent use of local clays by area potters and by their systems for refining it. After the raw clays were dried out, they were mixed as slips, passed through a screen or a series of screens, and then blended with other clays to make the potters’ custom clay bodies.

Mixing these materials as a slip allows them to be readily passed through screens and it also addresses the biggest issue when making any clay regardless of whether or not you’re using local materials—the difficulty of thoroughly mixing it. The simplest way to mix materials thoroughly is by blunging them together as a slip, but then you have all of this slip, and how are you supposed to dry it to a workable clay state? You could dry your slip on a plaster block, but plaster dries your clay unevenly, and if it’s already saturated with water from a previous round of slip drying, you have to wait until the plaster dries out.

The Solution?

Clay drying beds—or the gravity filter press, as I like to call it (1). Much like a traditional filter press would pump pressurized clay slip into a cloth, pushing water out through the cloth, not allowing the clay to pass through, and quickly leaving you with workable clay, the gravity filter press accomplishes the same result with just a little more time and far less technical equipment. Instead of pumping the slip in, you just pour the slip on top of a suspended cloth and watch as crystal clear water drips out the bottom (2). With a rudimentary wooden frame, some chicken wire, an old bed sheet, some plastic, a bucket, and a few thumbtacks, you’ll be thoroughly mixing and drying your slip or reclaim into a usable clay body like the pros in no time!

2 Henry Crissman pouring slip into his gravity filter press.

Many of the North Carolina potters had drying beds larger than 4×8 feet, but with limited space and resources, I built mine to stack on top of each other using the wood from a couple of old pallets. Their drying beds were often outside, with the draining water from the clay just falling to the ground. Being indoors, I stretched a sheet of plastic under mine that directs the water to drip into a bucket on the floor. The bed sheet I use has a standard thread count and it would work just fine as a single layer, but I’ve doubled it over for strength. The slip seems to dry most evenly when it is no deeper than 2 inches thick in the drying bed (3). With more heat and/or air circulation the process is sped up and you can more readily dry a deeper layer of slip.

This can be a great tool to use when making a fresh batch of clay or to reconstitute your reclaim. Now get out there, mix your clay bodies as a slip, maybe get some local clays involved, and enjoy your perfectly blended clay!

3 The gravity filter press in action. Water drips out of the slip and through the bedsheet, catches on the plastic, and drips into the bucket.

the author Henry James Haver Crissman currently resides in Alfred, New York, and is the studio manager at the Wellsville Creative Arts Center in Wellsville, NewYork.

Send your tip and tool ideas, along with plenty of images, to editorial@ceramicsmonthly.org. If we use your idea, you’ll receive a complimentary one-year subscription to CM!

Comments
  • Dear Henry Crissman,
    This is exactly what I have been looking for! Thank you for sharing this idea. I have a small studio and live in SD. I have used plaster table to dry my recycled clay but it is also the plaster table I wedge and do other work on. I have started harvesting my own clay and need to mix ball clay into it for plasticity. It’s a lot of work wedging when you add in the work of harvesting. I just mixed up my first batch of clay slurry and put it on my newly made “Gravity Filter Press”. I’m so excited. As a bonus… while taking care of some business in the bathroom I made the connection to use the shower stall that is never used! I have limited space and the year round outdoors is out of the question. (It’s 3 degrees for the high today. Can’t wait to see how it drys. Thank you, thank you, thank you.

  • does the moist come out quicker than on a plaster bat ? Is it a faster process than drying on plaster ? Thank you for your reply !

    • Hi Golly! I tried both way (i’ve been digging up my own clay and this part of process almost same) plaster bat is absolutely faster way but drying is not even. The surface touch the plaster dry but top of the slip still wet. And think this;if u use plaster u have to knead and i hate this part.Specially big amounts. If u use bed sheets drying will take more time but u ll have nice even moistured clay ball and u dont need to knead at all. No air bubbles,no tired arms! And i have to say this,u have to give time to ripen to clay. When i use bed sheet method my clay has more plasticity.

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend