Firing temperature : cone 8-11 | Surface texture : matte | Color : cream | Atmosphere: Oxidation/Neutral Reduction

Published in "Atmospheric Recipes," in the October 2018 issue of Ceramics Monthly. This recipe has been used by Susan McKinnon.


Click Image to Enlarge

Ingredients

Instructions

Mix all dry ingredients together, then divide into small quantities (use amount based on preference). Make Soda Mix burritos in wet newspaper and allow them to set after rolling. Using two layers of wet newsprint allows the mix to set with minimal cleanup.