Will and Kate Jacobson’s Naked Raku

Firing temperature : cone 05 | Surface texture : matte | Color : various | Atmosphere: Raku

Published in "From Oh No! to Oh Wow!" by Kate and Will Jacobson, in the Sep/Oct 2011 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Apply thin or thick over dry sacrificial or breakaway slip.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • James F.

    Haveused that recipe and only achieved white and black crackle with no color. How do you achieve the color that is shown on the website.

    • Karl N.

      From the article.. they use colored slips at greenware stage and the patterns you see there are their sort of sgraffito technique through the colored slips. Then it’s burnished prior-to bisque. The recipe for the above resist slip is used over the piece after it is bisqued.

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend