Firing temperature : cone 06 | Surface texture : glossy | Color : dark red | Atmosphere: Oxidation/Neutral Reduction

Published in "Successful Raku Firing" by George Juliano with Elizabeth Hudgins, in the Fall 1998 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This glaze looks best when applied thin. I generally dip the pot once in a thin mixture. The glaze has a dark cranberry luster in appearance. I place pieces glazed with Copper Luster in a lidded trash can filled with newspaper, since this seems to make the colors shine a bit brighter.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend