Ingredients

Instructions

Ferro frit #3110 provides the flux you need in the glaze for it to melt. In fact, at the raku temperature range, frits are complete glazes by themselves.

EPK kaolin, which is a clay containing alumina and silica, prevents a molten glaze from running down vertical surfaces.

Stains provide color to the base glaze.

Superpax is an opacifier that makes the clear, gloss, transparent base glaze an opaque, gloss white.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend