Yoko Sekino-Bove’s N502

Yoko Sekino-Bove’s N502

Firing temperature : cone 5 | Surface texture : glossy | Color : turquoise green | Atmosphere: Oxidation/Neutral

Published in "Expanding Your Palette in Mid-Range Firing" by Yoko Sekino-Bové, in the Jan 2011 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

The test batch for this glaze was 300g, with a tablespoon of epsom salts added as a flocculant.

Fire in an electric kiln, in an oxidation/neutral atmosphere.