Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

This recipe was shared by London Clay Art Centre in the February 2019 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

This recipe works well with Mason stains and oxides added for color. To test colorants, start with 0.25–2% of metallic oxide colorants, and 1–5% of Mason stains of other commercial stains. Susan Day and Beth Turnbull Morrish used this glaze on the outdoor mosaic at London Clay Art Centre in London, Ontario, Canada.