Wood Ash Glaze

Wood Ash Glaze

Firing temperature : cone 8 | Surface texture : matte to satin | Color : various | Atmosphere: Reduction

This recipe was shared by Hanako Nakazato in the June/July/August 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Ingredients

Instructions